Preparation of lamellar and hexagonal forms of mesoporous silica and zirconia by the neutral amine route: lamellar–hexagonal transformation in the solid state

Abstract

The chain length of the surfactant and the solvent composition are two of the factors that determine whether the lamellar or the hexagonal form of mesoporous SiO2(or ZrO2) is formed by the neutral amine route; a lamellar–hexagonal transformation occurs on removal of the amine from the former.

Article information

Article type
Paper

Chem. Commun., 1996, 2243-2244

Preparation of lamellar and hexagonal forms of mesoporous silica and zirconia by the neutral amine route: lamellar–hexagonal transformation in the solid state

N. Ulagappan, Neeraj, B. V. N. Raju and C. N. R. Rao, Chem. Commun., 1996, 2243 DOI: 10.1039/CC9960002243

To request permission to reproduce material from this article, please go to the Copyright Clearance Center request page.

If you are an author contributing to an RSC publication, you do not need to request permission provided correct acknowledgement is given.

If you are the author of this article, you do not need to request permission to reproduce figures and diagrams provided correct acknowledgement is given. If you want to reproduce the whole article in a third-party publication (excluding your thesis/dissertation for which permission is not required) please go to the Copyright Clearance Center request page.

Read more about how to correctly acknowledge RSC content.

Social activity

Spotlight

Advertisements